A rapid method for concentrating sedimentary organic matter for vitrinite reflectance analysis

Journal of Sedimentary Petrology
By:

Links

Abstract

The tecnique discussed in this paper utilizes crushing, high-speed blending, and ultrasonic treatment to mechanically disaggregate rock and release the sedimentary organic matter (OM) in a suitable heavy liquid. This new method can provide freeze-dried concentrated OM in approximately 8 to 24 hours (longer time is necessary for removing carbonate). Under optimal conditions, it is possible to concentrate the OM and prepare a hardened epoxy microscope slide in about 24 hours. Subsequent grinding, polishing, and drying allows microscopic examination of the organic concentrate the next day.

Suggested Citation

Barker, C., 1982, A rapid method for concentrating sedimentary organic matter for vitrinite reflectance analysis: Journal of Sedimentary Petrology, v. 52, no. 2, p. 663-664, https://doi.org/10.1306/212F7FEF-2B24-11D7-8648000102C1865D.

Publication type Article
Publication Subtype Journal Article
Title A rapid method for concentrating sedimentary organic matter for vitrinite reflectance analysis
Series title Journal of Sedimentary Petrology
DOI 10.1306/212F7FEF-2B24-11D7-8648000102C1865D
Volume 52
Issue 2
Year Published 1982
Language English
Publisher SEPM
Description 2 p.
First page 663
Last page 664
Additional publication details